1.4846不锈钢板
1.4846不锈钢板是德国材料号(Werkstoff-Nummer)体系中的高硅耐热不锈钢牌号,对应ASTM 310Si2、中国国标06Cr25Ni20Si2和欧标X12CrNiSi25-21。硅含量达1.50-2.50%,显著提高了抗渗碳性能,适用于渗碳炉、高温气氛炉等需要抵抗碳渗透的工况环境。
{"faq": [{"answer": "1.4846硅含量更高(1.50-2.50% vs ≤1.50%),抗渗碳性能更强,适合渗碳炉等含碳气氛环境。普通高温氧化环境选1.4845即可。", "question": "1.4846和1.4845有什么区别?"}, {"answer": "1.4846特别适合渗碳炉、碳氮共渗炉等需要抵抗碳渗透的环境,高硅含量形成致密氧化膜,阻止碳原子渗入。", "question": "1.4846适合用在什么环境?"}], "temp": "700~1200℃", "grade": "1.4846", "features": ["高硅含量", "抗渗碳", "耐高温"], "packaging": "标准出口包装:内衬塑料薄膜防潮,外用钢带捆扎,木托盘或木箱包装。可根据客户要求定制包装方式。", "standards": {"en": "X12CrNiSi25-21", "gb": "06Cr25Ni20Si2 (GB/T 1221)", "jis": "-", "uns": "S31009", "wnr": "1.4846", "astm": "A240/A240M 310Si2"}, "thickness": "0.5~60mm", "priceRange": "30,000 - 38,000", "stockSpecs": [{"width": "1000/1219mm", "length": "C(卷)", "thickness": "0.5~1.0mm"}, {"width": "1000/1219/1500mm", "length": "C(卷)/2000/2438mm", "thickness": "1.0~3.0mm"}, {"width": "1219/1500mm", "length": "2000/2438/6000mm", "thickness": "3.0~6.0mm"}, {"width": "1500/1800/2000mm", "length": "6000mm", "thickness": "6.0~20mm"}, {"width": "1500/1800/2000mm", "length": "6000mm", "thickness": "20~60mm"}], "application": "渗碳炉、高温气氛炉、热处理设备", "description": "1.4846不锈钢板是德国材料号(Werkstoff-Nummer)体系中的高硅耐热不锈钢牌号,对应ASTM 310Si2、中国国标06Cr25Ni20Si2和欧标X12CrNiSi25-21。硅含量达1.50-2.50%,显著提高了抗渗碳性能,适用于渗碳炉、高温气氛炉等需要抵抗碳渗透的工况环境。", "deliveryTime": "常规规格现货3-5天发货,非标规格定制10-20天", "certifications": ["ISO 9001:2015", "SGS 质量认证", "TUV 认证", "PED 认证", "DIN认证"], "surfaceTreatments": ["No.1(热轧退火酸洗)", "2B(冷轧退火酸洗)"], "physicalProperties": {"density": "7.98 g/cm³", "meltingPoint": "1398~1454℃", "specificHeat": "500 J/kg·K", "elasticModulus": "200 GPa", "thermalExpansion": "15.9 ×10⁻⁶/℃ (0~100℃)", "thermalConductivity": "14.2 W/m·K (100℃)", "electricalResistivity": "0.78 μΩ·m"}, "chemicalComposition": [{"content": "≤0.08%", "element": "C(碳)"}, {"content": "1.50~2.50%", "element": "Si(硅)"}, {"content": "≤2.00%", "element": "Mn(锰)"}, {"content": "24.00~26.00%", "element": "Cr(铬)"}, {"content": "19.00~22.00%", "element": "Ni(镍)"}, {"content": "≤0.030%", "element": "S(硫)"}, {"content": "≤0.035%", "element": "P(磷)"}], "applicationScenarios": [{"industry": "热处理", "equipment": "渗碳炉、碳氮共渗炉", "description": "高硅含量有效抵抗碳渗透,延长炉体寿命"}, {"industry": "化工行业", "equipment": "高温反应器、裂解炉", "description": "耐渗碳腐蚀,适合含碳气氛环境"}, {"industry": "新能源", "equipment": "锂电池正极材料烧结炉", "description": "高温烧结环境下抗渗碳、抗腐蚀,保障产品纯度"}, {"industry": "环保设备", "equipment": "危废焚烧炉、热解气化炉", "description": "耐高温渗碳气氛腐蚀,适用于固废处理高温设备"}], "mechanicalProperties": [{"value": "≥520", "property": "抗拉强度(MPa)"}, {"value": "≥205", "property": "屈服强度(MPa)"}, {"value": "≥40", "property": "延伸率(%)"}, {"value": "≤187", "property": "硬度(HB)"}], "processingPerformance": {"weldMethod": "TIG焊、MIG焊、手工电弧焊", "formability": "良好,可进行冷弯、热弯等加工", "weldability": "良好,需注意硅对焊接的影响", "heatTreatment": "固溶处理 1040~1150℃ 水冷", "machinability": "中等,硅含量较高时加工难度略增"}}